LF2010 is a hexene LLDPE with increased stiffness suitable for blown heavy duty films and shipping sacks. This material contains process aid for improved ease of extrusion, and can be blended with LDPE for strength property enhancements. Test specimens for blown film: nominal thickness 1.0 mils fabricated at 2.5:1 BUR, 50 mil die gap, 440 ° F, 9 Ibs/hr/ in. This product has some 21 CFR clearances. Application/Uses: - Bags and sacks- Agricultural films- Heavy duty bags and sacks- Co-extruded structures. Samples tested at 23°C and 50% RH. Information provided by Westlake Chemical Corporation. |