MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI Latiohm 80-05 CNT GCE/500 PPS, Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Carbon nanotubes. Glass fibers / Mineral filler.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.812 g/cc
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa
Elongation at Break 0.50 %
Tensile Modulus 15700 MPa
Charpy Impact Unnotched 20.0 kJ/m²
Charpy Impact, Notched 3.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10000 ohm-cm
Surface Resistance 3000 ohm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 280 °C
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
Vicat Softening Point 255 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 - 310 °C
Mold Temperature 120 - 130 °C
Drying Temperature 130 - 150 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Unifrax FyreWrap® Cable Insulation
TIMET TIMETAL® 21S Titanium + Silicon Carbide Fiber Composite
Momentive Performance Materials "PG" Pyrolytic Graphite
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF

PLATH9951 / 177647

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.