MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Clearflex® FH 50 Linear Medium Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes: Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.

Films manufactured with Clearflex FH 50 are characterized by a good balance between toughness and rigidity, have high temperature resistance together with optimum sealing properties.

Main Applications: Due to its mechanical properties and excellent processability, Clearflex FH 50 is recommended in coextrusion for the production of film having good rigidity. Moreover, its very low gel content makes the resin ideal for lamination.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.936 g/ccISO 1183
Thickness 10.0 - 50.0 micronsRecommended
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 16.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPaISO 527-3
Film Elongation at Break, MD 650 %ISO 527-3
Film Elongation at Break, TD 750 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 0.8152 g/micronISO 6383-2
Elmendorf Tear Strength, TD 10.19 g/micronISO 6383-2
Dart Drop Test 50.0 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 35.0 MPaISO 527-3
Film Tensile Strength at Break, TD 25.0 MPaISO 527-3
1% Secant Modulus, MD 450 MPaISO 527-3
1% Secant Modulus, TD 500 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 128 °CInternal method
Vicat Softening Point 117 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 18 %ISO 14782
Gloss 55 %45°; ASTM D2457
Transmission, Visible 90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene
LyondellBasell Petrothene® NA951080 Low Density Polyethylene
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene
ICO Polymers ICORENE™ 110-1016 LMDPE Rotational Molding Resin

PENG062 / 124456

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.