Mirel™ P1003 is a general purpose injection molding material with high modulus. Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and closures, and disposable items such as forks, spoons, knives, tubs, trays, jars, and consumer product applications. About Mirel Bioplastics Mirel is a family of bioplastic materials that have physical properties comparable to petroleum-based resins, yet are both biobased and biodegradable in natural soil and water environments, home composting systems, and industrial composting facilities, where these facilities are available. The rate and extent of Mirel's biodegradablility will depend on the size and shape of the articles made from it. However, like nearly all bioplastics and organic matter, Mirel is not designed to biodegrade in conventional landfills. Telles is a joint venture between Metabolix and Archer Daniels Midland Company. |