MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem HS5502 Blown Molding and Injection Blown Molding High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade; High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description: HS5502 is a high density polyethylene, copolymer. Offers good processability and bottles produced have excellent stiffness.

Application: Blow Molded Small Volume: Food, lubricant oils and pharmaceutical packing; Toys; Braskem does not recommend the use of HS5502 for the production of films.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D792
ESCR 100% Igepal® >= 20 hour
@Temperature 50.0 °C
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
ESCR 10% Igepal® 10 hour
@Temperature 50.0 °C
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Melt Flow 0.35 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 32 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPaASTM D638
Flexural Modulus, 1% Secant 1350 MPaASTM D790
Izod Impact, Notched 150 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Feed Temperature 185 °C
Die Temperature 195 °C
Mold Temperature 5.00 - 25.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem GM5340PR High Density Polyethylene
Braskem GF4950 HDPE Blow Molding Polyethylene Copolymer
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer
Braskem ES6007 Blown Molding and Injection Blown Molding High Density Polyethylene
Braskem ES6004 Blown Molding High Density Polyethylene

PBRASK2090 / 199971

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.