MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Nabaltec APYRAL® AOH 180DS AlO(OH) Boehmite  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: APYRAL® AOH 180 is selected due to its high specific surface area and well defined grain size distribution, resulting in a constant reactivity. In the field of halogen-free mineral flame retardancy, APYRAL® AOH 180 can be used in polymeric applications exceeding processing temperatures of 200°C. Converts to gamma-alumina after activation at 550°C/3h.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 g/cc
Brightness 98 %
@Wavelength 457 nm
Whiteness
Moisture Absorption at Equilibrium 0.40 %
Loss On Ignition 17 %
@Temperature 105 - 1000 °C
Particle Size 0.60 µmMedian Grain Diameter
 >= 45 µm0.01% greater than
Specific Surface Area 0.18 m²/gBET, values after activation at 550 °C/3h
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1250 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.020 %
Na2O 0.40 %
SiO2 0.020 %
 
Descriptive Properties
Crystal StructureBoehmite
Gibbsite Max. %0.6
Pore Volume cc/g0.1Values after activation at 550 °C/3h

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GBC Grade 85 Alumina
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
CeramTec 771 94% Alumina (Al2O3)

CNABAL22 / 54547

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.