MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon® NXT 85 Chemically Modified Free-Flow Granular Fluoropolymer Molding Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: DuPont™ Teflon® PTFE NXT85 is a free-flowing, pelletized, chemically modified granular resin (its equivalent fine-cut resin is Teflon® NXT 75). It provides superior processing characteristics in addition to properties of chemically modified resins. This resin offers excellent powder flow and high bulk density.

When properly processed, Teflon® PTFE NXT85 exhibits the superior properties typical of the fluoropolymer resins: nonaging characteristics, chemical inertness, heat resistance, toughness and flexibility, low coefficient of friction, nonstick characteristics, negligible moisture absorption, and weather resistance. In addition to typical properties of fluoropolymers, this chemically modified resin offers weldability, improved resistance to deformation under load, increased resistance to permeation of chemicals, and a higher dielectric breakdown strength. It provides a high degree of weldability for applications where the use of elevated temperature and pressure are limited.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.17 g/ccASTM D4894
Apparent Bulk Density 0.780 g/ccASTM D4894
Particle Size 400 µmAverage diameter; ASTM D4894
Deformation 3.5 %14 MPa load, 23°C; ASTM D621-A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 28.0 MPaASTM D4894
Elongation at Break 400 %ASTM D4894

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® NXT 75 Fluoropolymer Resin Modified PTFE Granular Molding Resin
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Chemours Teflon® NXT 70 Fluoropolymer Resin Modified PTFE Granular Molding Resin
Chemours Teflon® FEP CX5010 Fluoropolymer Resin
Chemours Teflon® 807-N PTFE granular molding resin

PDU9260 / 104554

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.