MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Manifattura Cattaneo PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.

Information provided by Manifattura Cattaneo s.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0647 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.050 %
@Temperature 23.0 °C
0.050 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation 0.050 %0.050 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ISO 2039-2
Tensile Strength at Break 30.0 - 50.0 MPa4350 - 7250 psiISO 527
Tensile Strength, Yield 50.0 - 55.0 MPa7250 - 7980 psiISO 527
Elongation at Break 20 - 60 %20 - 60 %ISO 527
Tensile Modulus 2.30 GPa334 ksiISO 527
Flexural Strength 74.0 MPa10700 psi
Flexural Modulus 2.25 GPa326 ksiISO 178
Compressive Yield Strength 17.0 MPa
@Strain 1 %
2470 psi
@Strain 1 %
ISO 604
Poissons Ratio 0.350.35
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
Coefficient of Friction, Dynamic 0.20 - 0.350.20 - 0.35on polished steel; MPC Test
Coefficient of Friction, Static 0.20 - 0.400.20 - 0.40on polished steel; MPC Test
K Factor (Wear Factor) 0.600.60µm/s. PV = 0.1 MPa-m/s; max P = 25 MPa; MPC Test
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+16 ohm-cm5.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60094
Dielectric Constant 7.5
@Frequency 1e+6 Hz
7.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 - 30.0 kV/mm
@Thickness 2.00 mm
508 - 762 kV/in
@Thickness 0.0787 in
IEC 60243
Dielectric Loss Index 0.15
@Frequency 1e+6 Hz
0.15
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 125 - 140 µm/m-°C
@Temperature 23.0 - 100 °C
69.4 - 77.8 µin/in-°F
@Temperature 73.4 - 212 °F
ASTM D696
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDOM 52612
Maximum Service Temperature, Air 150 °C302 °F
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FISO 75
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 V-0V-0
Oxygen Index 44 %44 %ISO 4589
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorWhite
UV ResistanceY

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CENTROPLAST CENTROFLON Polyvinylidene fluoride
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
Murtfeldt Murinyl® Polyvinylidinefluoride
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded

PMANIF909 / 156189

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.