MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAFAC® AAP Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: AMYL ACID PHOSPHATE; ORGANIC ACID PHOSPHATE

CAS: 71-41-0, 7664-38-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAFAC© AAP imparts excellent extreme pressure and anti-wear properties in lubricating oils and greases.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 - 1.11 g/cc0.0387 - 0.0401 lb/in³RP-0134
pH <= 2.5<= 2.5at 10%
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 270 - 280270 - 280[mg KOH/g], #1; RP-0427
 400 - 450400 - 450[mg KOH/g], #2; RP-0427
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.30 %<= 0.30 %RP-0327
 
Descriptive Properties
AppearanceColorless to Pale Yellow LiquidRP0064
Color<500APHA, RP-0549
CompositionAmyl Dihydrogen Phosphate40-55%, RP-0427
 Diamyl Hydrogen Phosphate40-57%, RP-0427
 Free Amyl Alcohol<8%, RP-8086
 Free Phosphoric Acid<1%, RP-8086
 Phosphorus14.5-15.5%, RP-0427
Surfactant Content>90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® ARB/70 Surfactant
Solvay RHODAFAC® ARB/90 Surfactant
Solvay RHODAFAC® BN-936/S Surfactant
Solvay RHODAFAC® PA23 Surfactant
Solvay RHODAFAC® RA-600 E Surfactant

WRHOD346 / 137577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.