MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFIL PA6 GF30 black - 1,75 mm - Filament Nylon 6, 30% Glass Fiber Reinforced
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes:
  • high strength
  • high dimensional stability
  • good weldable and bondable
  • good heat deflection temperature
  • resistant to many oils, greases and fuels
Target Industries:
  • electronics
  • automotive industry
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
Moisture Absorption 0.300 %0.300 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 72.0 MPa10400 psi5mm/min, Orientation XY; DIN EN ISO 527-2
Elongation at Break 5.0 %5.0 %5mm/min, Orientation XY; DIN EN ISO 527-2
Modulus of Elasticity 5.20 GPa754 ksi5mm/min, Orientation XY; DIN EN ISO 527-2
Flexural Strength 115 MPa16700 psi2mm/min, Orientation XY; DIN EN ISO 178
Flexural Modulus 4.46 GPa647 ksi2mm/min, Orientation XY; DIN EN ISO 178
Flexural Strain at Break 6.0 %6.0 %2mm/min, Orientation XY; DIN EN ISO 178
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C33.3 µin/in-°FDIN EN ISO 11359-1;2
Melting Point 220 °C428 °FDIN EN ISO 11357
Maximum Service Temperature, Air 100 °C212 °Flong term
 180 °C356 °Fshort term
Glass Transition Temp, Tg 60.0 °C140 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °FBuild chamber temperature
 80.0 - 140 °C176 - 284 °FPrint bed temperature
Nozzle Temperature 260 - 290 °C500 - 554 °FDiameter: 0,4 mm
Melt Temperature <= 300 °C<= 572 °F
Drying Temperature 80.0 °C176 °F
Dry Time 8.00 hour8.00 hour
 
Descriptive Properties
Colorblack opaque
Fan speed0-20%
Print speed30-50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO1260 / 319188

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.