SB-30 is an unground ATH, commonly known as aluminum hydroxide used to suppress flame and smoke in plastics, rubber and cellulosics. SB-30 is an off-white product that can be used in most applications where a coarse alumina trihydrate is required. A complete range of surface modifications is available to aid processing and enhance physical properties. These include silanes, stearates and wetting agents. Technical service is available.Information provided by J.M. Huber Corporation |