System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
MetalTek AGMA CL A UNS C90800 Gear Bronze
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Bronze
Material Notes:
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.
Applications: Worm gears, steel mill nuts
Information provided by MetalTek
Cast UNS C90800; Cast Grade C90800; Cast ASTM B427, B505
Key Words:
Tin Bronze
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
8.67
g/cc
0.313
lb/in³
Based on UNS number
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
95
95
500 kg
Tensile Strength, Ultimate
>=
345
MPa
>=
50000
psi
Tensile Strength, Yield
>=
195
MPa
>=
28300
psi
Elongation at Break
>= 12 %
>= 12 %
Component Elements Properties
Metric
English
Comments
Copper, Cu
87.8 %
87.8 %
Phosphorus, P
0.20 %
0.20 %
Tin, Sn
12 %
12 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
MetalTek AGMA CL B UNS C91700 Gear Bronze
MetalTek MTEK 102-N Cast UNS C92900 Gear Bronze
MetalTek MTEK 65+Ni UNS C91600 Gear Bronze
MetalTek MTEK 78-7-15 HI LEAD Cast UNS C93800 Bearing Bronze
MetalTek MTEK 83-7-7-3 Cast UNS C93200 Bearing Bronze
NMETEK015 / 18265
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.