MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman MPK, UHP Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 107-87-9

Product Description: Eastman™ MPK (Methyl Propyl Ketone), UHP (Ultra High Purity), is a medium evaporating, urethane grade solvent. It is an active solvent for most synthetic resins including acrylics, polyesters, cellulosics, epoxies, vinyls, and alkyds. Its high solvency, low density, and medium evaporation rate make it attractive as a letdown solvent for high-solids air-dry resins used in low VOC alkyd and polyester/urethane coatings. It is used in gravure printing inks and also provides excellent performance for a wide range of cleaning and surface preparation applications for the transportation industry.

Application/Uses:

  • Cleaners - Metal prep Hand Wipes, Ink Processes, and Light Degreaser
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
  • Graphic Arts - Gravure Printing Inks
  • Letdown Solvent - High-Solids Resins
Key Attributes:
  • Excellent solvent activity
  • High dilution ratio
  • Inert - Nonfood use
  • Low density
  • Medium evaporation rate
  • Meets Aerospace NESHAP compliance
  • Non-HAP
  • Non-SARA
  • REACH compliant
  • Readily biodegradable

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.807 g/cc
Vapor Pressure 0.0366 atm
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.020
 
Thermal PropertiesOriginal ValueComments
Melting Point -84.0 °CFreezing Point
Boiling Point 103 °CInitial, @ 760 mm Hg
Flash Point 10.0 °CTag Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.39
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5250 / 222444

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.