MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® C665 Copper Foil Backing Acrylic Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoplastic; Acrylic (PMMA)

Material Notes: CHR® C665 is manufactured from electrically deposited copper foil backing with acrylic adhesive.

Features/Benefits: The copper foil and adhesive of C665 are both electrically conductive and the release liner aids in die cutting. C665 tapes offers solvent resistance. C665 can meet Underwriters Laboratories recognized component program Guide OANZ2, File E51201 and UL510 flame retardant specifications.

Applications: CHR® C665 tape is designed for conductivity through the entire construction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Outgassing - Total Mass Loss 0.070 %
Collected Volatile Condensable Material 0.020 %
 
Mechanical PropertiesOriginal ValueComments
Tear Strength 70.2 pliTensile Strength
Peel Strength 0.380 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.010 ohm-cmohms/in
Surface Resistance 0.0065 ohmohms/in
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 374 °F
Minimum Service Temperature, Air -99.4 °F
 
Descriptive Properties
ColorCopper

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics THERMATTACH® T412 Thermally Conductive Attachment Tape
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 20 µm)
3M 3513 Copper Foil Tape
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
3M 3324 Copper Foil Tape

PSTGQZ470 / 68984

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.