MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Eastek™ 4100 Polyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Eastek 4100 is a high-performance polyester resin for polyurethane hot melt adhesive applications. Eastman Eastek 4100 resin is designed to improve cross linking, increase Tg, and improve formulation flexibility. These attributes enable greater productivity, application consistency, long-term durability, and expanded application space for woodworking, packaging, assembly, and automotive applications.

Applications

  • Adhesives
  • Adhesives/sealants-b&c
Key Attributes
  • Excellent green strength
  • Good heat and hydrolytic stability
  • High Mw with functional hydroxyl group
  • High Tg
  • Superior adhesion to metal substrates

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Test 36.0 cm³/g0.360 dl/gInherent
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 4.004.00[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 78.0 °C172 °F
 
Descriptive Properties
FormSolid Pellet
Hydroxyl Number15 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4131 / 323754

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.