MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV160 White Adhesive Sealant, Non-Corrosive Pourable
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive protection of printed circuit boards from dirt, dust, moisture, and solvents. Coat contact points. Seal exposed wires. Cushion between plastics and metals, Thin-section potting.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25
Tensile Strength, Ultimate 1.86 MPa
Elongation at Break 230 %
Adhesive Bond Strength 0.690 MPaTypical lap shear
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 205 °CContinuous useful temperature.
Minimum Service Temperature, Air -60.0 °CContinuous useful temperature.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 25.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant
Momentive Performance Materials TSE3941 Flame Retardant Adhesive Sealant, White
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White
Momentive Performance Materials IS802 White Adhesive Sealant, General Purpose Paste
Momentive Performance Materials IGS3703 Insulating Glass Sealant

PZZGE920 / 40474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.