MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
OCSiAl TUBALL™ MATRIX 808 Graphene Nanotube Concentrate
Categories: Carbon; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TUBALL™ MATRIX 808 beta is versatile conductive additive for compounding of TPU, filled PPS, ABS, PC, PC-ABS, PA, GF PA. TUBALL™ MATRIX 808 beta is available in coarse powder form as TUBALL™ MATRIX 808 beta PWD. TUBALL™ is a unique graphene nanotube additive from OCSiAl that provides electrical conductivity at ultralow dosage with minimal impact on the rheological and mechanical properties of the host matrix.

Benefits: TUBALL™ MATRIX 808 beta only requires an ultra-low dosage starting from just 1 wt.%, Minimal influence on mechanical properties, Ensures permanent and uniform electrical properties without “hot spots”, Without a significant increase in viscosity or density of the host material.

Information provided by OCSiAl

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Softening Point 65.0 °CASTM D3461
Flash Point >= 270 °CISO 2592
 
Descriptive Properties
CarrierFatty Acid, Ester of Polyol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOCSIAL920 / 305659

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.