MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam 2460 Antifoam concentrate
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam 2460 is an APEO-free organic antifoam concentrate based on mineral oil.

Application: TEGO® Antifoam 2460 is designed for the use as process aid in the water-based polymerization of SBR/ NBR rubber materials. However, for the defoaming of SBR emulsions as used in adhesives and paper coatings, we rather recommend to use the specialized defoamers TEGO® Antifoam 2290 and 2291.

Properties / Benefits: Unlike conventional defoamers, TEGO® Antifoam 2460 was specifically developed to avoid premature coagulation. This allows for less cleaning of the reaction vessel and the demonomerization column while the TEGO® Antifoam 2460 does not hinder the coagulation stage. Test with the customer specific emulsions are recommended.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/cc
Viscosity 50 - 120 cP
 
Descriptive Properties
Appearancegrey, turbid liquid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omya OMYACARB® 15 - LU Calcium Carbonate
Omya SNOWHITE® 17 - PT Calcium Carbonate
Omya SNOWHITE® 350 - PT Calcium Carbonate
Omya SNOWHITE® 3 - PT Calcium Carbonate
Omya SNOWHITE® 12-40 - PT Calcium Carbonate

PEVONIL549 / 196753

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.