MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and conventional molding machines

Applications: Pentfoam 321F is particularly well suited for hte manufacture of EPS part products, with part wall thickness above approximately 10 MM. This grade is also widely used for production of insulation boards and panel, block molded or produced in continuous molding machines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0140 - 0.0150 g/cc
 0.0160 - 0.0250 g/ccmolding density range
Bead Size 0.630 - 1.12 mm
Maximum Moisture Content 0.20
 
Chemical PropertiesOriginal ValueComments
Blowing Agent Content >= 5.8 %
 
Mechanical PropertiesOriginal ValueComments
K Factor (Wear Factor) 56 - 58

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical R160 EPS, Flame Retardant
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
LG Chemical R320 EPS, Flame Retardant
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene

PIRPC020 / 83997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.