MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® Care M40 G PEEK, Medical Device Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment. VESTAKEEP® Care M40 G is a high viscosity, unreinforced polyether ether ketone for injection molding and extrusion. The semi-crystalline polymer features superior thermal and chemical resistance.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Opaque
Resistance to: Heat (thermal stability), Fire / burn, Hydrolysis / hot water, Fatigue resistance, Oil / fuels
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Applications: Encapsulation
Special Characteristics: Phosphorus-free, PTFE-free, Semi-crystalline
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Water Absorption 0.400 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00900 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cmISO 294-4, 2577
Melt Flow 11.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 96.0 MPaISO 527
Tensile Strength, Yield 96.0 MPaISO 527
Elongation at Break 30.0 %Nominal; ISO 527
Elongation at Yield 5.00 %ISO 527
Tensile Modulus 3500 MPaISO 527
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm?V; IEC 62631-3-1
Dielectric Constant 2.80IEC 62631-2-1
Comparative Tracking Index 200 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Vicat Softening Point 305 °C
@Load 5.10 kg
50 K/h; ISO 306
 335 °C
@Load 1.02 kg
50 K/h; ISO 306
Flammability, UL94 V-0
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 °CInjection Molding; ISO 294
Mold Temperature 180 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secInjection Molding; ISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7845 / 324977

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.