MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLOY™ FR CM6140 PC+ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CM6140 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, non chlorinated/brominated mineral-filled flame retardant grade. It features high modulus, good flow, ductility and low warpage. It has a UL94 V0@0.8mm and 5VB@1.5mm flame rating and is a good candidate for thin wall applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Water Absorption 0.090 %0.090 %23°C/sat; ISO 62
 0.10 %0.10 %24 hours; ASTM D570
Moisture Absorption 0.0100 %0.0100 %50% RH, 24 hrs; ASTM D570
 0.0100 %0.0100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0050 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  14 g/10 min
@Load 5.00 kg,
Temperature 220 °C
14 g/10 min
@Load 11.0 lb,
Temperature 428 °F
cm³/10 min; ISO 1133
 17.5 g/10 min
@Load 2.16 kg,
Temperature 260 °C
17.5 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi5 mm/min; ASTM D638
 50.0 MPa7250 psi5 mm/min; ISO 527
Tensile Strength, Yield 65.0 MPa9430 psi5 mm/min; ASTM D638
 65.0 MPa9430 psi50 mm/min; ASTM D638
Elongation at Break 15 %15 %50 mm/min; ISO 527
 100 %100 %5 mm/min; ASTM D638
Elongation at Yield 3.5 %3.5 %5 mm/min; ISO 527
 4.0 %4.0 %5 mm/min; ASTM D638
Tensile Modulus 3.20 GPa464 ksi1mm/min; ISO 527
 3.50 GPa508 ksi5 mm/min; ASTM D638
Flexural Yield Strength 97.0 MPa14100 psi2 mm/min; ISO 178
 100 MPa14500 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.30 GPa479 ksi1.3 mm/min, 50 mm span; ASTM D790
 3.45 GPa500 ksi2 mm/min; ISO 178
Izod Impact, Notched 2.00 J/cm3.75 ft-lb/inASTM D256
 0.880 J/cm
@Temperature -30.0 °C
1.65 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*3; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 J36.9 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.68e+16 ohm-cm2.68e+16 ohm-cmASTM D257
Surface Resistance 3.54e+15 ohm3.54e+15 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
@Thickness 6.40 mm
207 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 83.0 °C
@Thickness 3.20 mm
181 °F
@Thickness 0.126 in
unannealed; ASTM D648
 89.0 °C
@Thickness 6.40 mm
192 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 91.0 °C196 °FRate B/50; ASTM D1525
 98.0 °C208 °FRate B/50; ISO 306
 102 °C216 °FRate B/120; ISO 306
Flammability, UL94  V-1
@Thickness 0.600 mm
V-1
@Thickness 0.0236 in
UL 94
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL 94
 5VB
@Thickness 1.50 mm
5VB
@Thickness 0.0591 in
UL 94
Glow Wire Test  800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
 850 °C
@Thickness 1.00 mm
1560 °F
@Thickness 0.0394 in
IEC 60695-2-13
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °FInjection Molding
Zone 1 275 - 300 °C527 - 572 °F
Zone 2 275 - 300 °C527 - 572 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 275 - 300 °C527 - 572 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 90.0 °C194 °FInjection Molding
Dry Time >= 4.00 hour>= 4.00 hourInjection Molding
Moisture Content 0.040 %0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10790 / 244257

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.