MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Nordel® IP 3640 EPDM Hydrocarbon Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: This is an amorphous and low-diene containing ethylene-propylene terpolymer (EPDM) suitable for heat resistant peroxide cured moldings. NDR 3640.00 can be blended with butyl rubber to improve processing and vulcanizate properties of automotive and bicycle tire innertubes. NDR 3640.00 is a developmental product in bale form.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³ASTM D297
Volatiles <= 0.40 %<= 0.40 %Total Volatiles; DuPont Dow PQ-E-007
Mooney Viscosity 40
@Temperature 125 °C
40
@Temperature 257 °F
ML 1 + 4; ASTM D1646
Ash <= 0.10 %<= 0.10 %ASTM D5667
 
Descriptive Properties
ENB1.8 mass%ASTM D6047
Ethylene55 mass%ASTM D3900
Molecular Weight DistributionMediumDuPont Dow PQ-E-034 and 036
Product FormBale
Propylene43.2 mass%ASTM D3900
Residual Transition MetalMax 10 ppmDuPont Dow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 3430 EPDM Hydrocarbon Rubber
Dow Nordel® IP 3670 EPDM Hydrocarbon Rubber
Dow Nordel® IP 3720P EPDM Hydrocarbon Rubber
Dow Nordel® IP 3745P EPDM Hydrocarbon Rubber
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber

PDVG04 / 34124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.