MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.

Features: Available in cartridges with a static mixer and in tins; Easy to mix; Excellent high shear strength and very high peel properties; Corrosion-inhibiting; Toughened; Non-slump characteristic to 3mm thickness; Gap filling; Glue line control; Service temperature up to 100°C/212°F.
Applications: Metal, honeycomb and fibre-reinforced composite bonding applications; Structural repair; Bonding inserts and ferrules; Bonding aluminum and composite edge members; Fabrication of honeycomb sandwich panels using the cut and fold technique.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
@Temperature 25.0 °C
Part B; ASTM D1622
 1.11 g/cc
@Temperature 25.0 °C
Mixed; ASTM D1622
 1.15 g/cc
@Temperature 25.0 °C
Part A; ASTM D1622
Viscosity 4000 - 8000 cP
@Temperature 25.0 °C
Part B; 0.50mm Gap, 40mm Parallel Plate, Strain = 0.01%; Bohlin Rheometer
 80000 - 90000 cP
@Temperature 25.0 °C
Part A; 0.50mm Gap, 40mm Parallel Plate, Strain = 0.01%; Bohlin Rheometer
 80000 - 100000 cP
@Temperature 25.0 °C
Mixed; 0.50mm Gap, 40mm Parallel Plate, Strain = 0.01%; Bohlin Rheometer
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77
@Temperature 22.2 °C
Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry; ISO R868
 79
@Temperature 22.2 °C
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ISO R868
Tensile Strength, Yield 1.073 ksi
@Temperature 22.2 °C
Flatwise Tensile, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-4
 1.218 ksi
@Temperature 22.2 °C
Flatwise Tensile, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-4
 3.988 ksi
@Temperature 22.2 °C
Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry; ISO R527
 5.802 ksi
@Temperature 22.2 °C
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ISO R527
Elongation at Break 2.47 %
@Temperature 22.2 °C
Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry; ISO R527
 5.53 %
@Temperature 22.2 °C
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ISO R527
Tensile Modulus 251 ksi
@Temperature 72.0 °C
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ISO R527
 291 ksi
@Temperature 72.0 °C
Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry; ISO R527
Compressive Yield Strength 1.45 ksi
@Temperature 60.0 °C
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ASTM D695
 1.45 ksi
@Temperature 60.0 °C
Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry; ASTM D695
 5.149 ksi
@Temperature 22.2 °C
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ASTM D695
 6.889 ksi
@Temperature 22.2 °C
Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry; ASTM D695
Poissons Ratio 0.53Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry
 0.68Cured Neat Resin Property, 5 days @ 22°C/72°F, Conditioning: Dry
Shear Strength 1.001 ksi
@Temperature 100 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-1
 1.624 ksi
@Temperature 100 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-1
 2.35 ksi
@Temperature 80.0 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-1
 2.364 ksi
@Temperature 40.0 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: 60°C / 140°F - 95% RH - 30 Days; EN2243-1
 2.538 ksi
@Temperature 40.0 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: 60°C / 140°F - 95% RH - 30 Days; EN2243-1
 3.307 ksi
@Temperature 60.0 °C
Tensile Lap Shear, 1 hour @ 120°C/248°F, Conditioning: Dry; EN2243-1
 3.466 ksi
@Temperature -55.0 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-1
 3.481 ksi
@Temperature 80.0 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-1
 3.742 ksi
@Temperature 60.0 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-1
 4.305 ksi
@Temperature 60.0 °C
Tensile Lap Shear, 1 hour @ 100°C/212°F, Conditioning: Dry; EN2243-1
 4.917 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: 60°C / 140°F - 95% RH - 30 Days; EN2243-1
 5.12 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Salt Spray 2000 hours; EN2243-1
 5.149 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Salt Spray 2000 hours; EN2243-1
 5.163 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: 60°C / 140°F - 95% RH - 30 Days; EN2243-1
 5.482 ksi
@Temperature 60.0 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-1
 5.526 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 1 hour @ 120°C/248°F, Conditioning: Dry; EN2243-1
 5.99 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-1
 6.28 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 1 hour @ 100°C/212°F, Conditioning: Dry; EN2243-1
 6.759 ksi
@Temperature 22.2 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-1
 7.092 ksi
@Temperature -55.0 °C
Tensile Lap Shear, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-1
Peel Strength 8.00 pli
@Temperature 100 °C
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2
 9.00 pli
@Temperature 100 °C
Bell Peel, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-2
 29.0 pli
@Temperature 80.0 °C
Bell Peel, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-2
 32.0 pli
@Temperature 80.0 °C
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2
 48.0 pli
@Temperature 60.0 °C
Bell Peel, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-2
 53.0 pli
@Temperature 22.2 °C
Bell Peel, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-2
 71.0 pli
@Temperature 60.0 °C
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2
 75.0 pli
@Temperature 22.2 °C
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 109 °FTg onset, 60°C/140°F-95%RH, 30days; Cured Neat Resin Property, 5 days @ 22°C/72°F
 111 °FTg onset, 60°C/140°F-95%RH, 30days; Cured Neat Resin Property, 1 hour @ 70°C/158°F
 127 °FTg tan d, 60°C/140°F-95%RH, 30days; Cured Neat Resin Property, 5 days @ 22°C/72°F
 129 °FTg tan d, 60°C/140°F-95%RH, 30days; Cured Neat Resin Property, 1 hour @ 70°C/158°F
 138 °FTg onset, Dry, Cured Neat Resin Property, 5 days @ 22°C/72°F
 158 °FTg tan d, Dry, Cured Neat Resin Property, 5 days @ 22°C/72°F
 162 °FTg onset, Dry, Cured Neat Resin Property, 1 hour @ 70°C/158°F
 192 °FTg tan d, Dry, Cured Neat Resin Property, 1 hour @ 70°C/158°F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 min
@Temperature 120 °C
EN 2243-1
 5.00 min
@Temperature 100 °C
EN 2243-1
 20.0 min
@Temperature 70.0 °C
EN 2243-1
 300 min
@Temperature 40.0 °C
EN 2243-1
 4320 min
@Temperature 22.0 °C
EN 2243-1
Pot Life 60 min
@Temperature 25.0 °C
100g; ASTM D2471-71
 
Descriptive Properties
Climbing Drum Peel (in-lb/3in)6972°F; EN2243-3; 5 days @ 22°C/72°F, Conditioning: Dry
 7272°F; EN2243-3; 1 hour @ 70°C/158°F, Conditioning: Dry
ColorBluePart B
 GreenMixed
 YellowPart A
Handling Strength (MPa)1.522°C; EN 2243-1; After 5 hours
 18.522°C; EN 2243-1; After 7 hours
Insert Shear Strength (lb)104°F; 1 hour @ 70°C/158°F, Conditioning: 70°C/15°8F-70%RH, equilibrium; AIRBUS S360M1M0006000
 104°F; 5 days @ 22°C/72°F, Conditioning: 70°C/15°8F-70%RH, equilibrium; AIRBUS S360M1M0006000
 72°F; 1 hour @ 70°C/158°F, Conditioning: Dry; AIRBUS S360M1M0006000
 72°F; 5 days @ 22°C/72°F, Conditioning: Dry; AIRBUS S360M1M0006000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Abatron AboCast 8110-5/AboCure 8110-1 Flexible Epoxy
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements

PHEXC476 / 99295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.