MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Ultimaker PLA Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Description: Ultimaker PLA filament provides a no-hassle 3D printing experience thanks to its reliability and good surface quality. Our PLA is made fromorganic and renewable sources. It’s safe, easy to print with, and it serves awide range of applications for both novice and advanced users

Key features: Good tensile strength and surface quality, easy to work with at high print speeds, user-friendly for both home and office environments, PLA allows the creation of high-resolution parts. There is a wide range of color options available

Applications: Household tools, toys, educational projects, show objects, prototyping, architectural models, as well as lost casting methods to create metal parts

Non-suitable for: Food contact and in vivo applications. Long term outdoor usage or applications

Information provided by Ultimaker

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D1505
Filament Diameter 2750 - 2950 µm2750 - 2950 µm
Melt Flow 6.09 g/10 min
@Load 2.16 kg,
Temperature 210 °C
6.09 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Tensile Strength at Break 45.6 MPa6610 psi50 mm/min; ISO 527
Tensile Strength, Yield 49.5 MPa7180 psi50 mm/min; ISO 527
Elongation at Break 5.2 %5.2 %50 mm/min; ISO 527
Elongation at Yield 3.3 %3.3 %50 mm/min; ISO 527
Tensile Modulus 2.3465 GPa340.33 ksi1 mm/min; ISO 527
Flexural Strength 103 MPa14900 psiISO 178
Flexural Modulus 3.15 GPa457 ksiISO 178
Izod Impact, Notched (ISO) 5.10 kJ/m²2.43 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
ASTM D150-11
Dissipation Factor 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
ASTM D150-11
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 - 160 °C293 - 320 °FISO 11357
Glass Transition Temp, Tg 60.0 °C140 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PULTIMK000 / 281739

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.