MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Non-halogen

Characteristics:

  • Impact resistant
  • Heat resistant
  • Flame retardant
  • Dimensional stability
  • Processability

Applications:

  • Cellular phone
  • Monitor housing
  • Coffee maker
  • Hair dryer
  • O/A part

All information provided by Samyang

Key Words: PC, ABS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.118 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Yield 58.8 MPa8530 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Flexural Yield Strength 78.5 MPa11400 psiASTM D790
Flexural Modulus 2.16 GPa313 ksiASTM D790
Izod Impact, Unnotched 4.41 J/cm
@Thickness 3.17 mm
8.27 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.00e+16 ohm-cm9.00e+16 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm762 kV/inASTM D149
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 sec120 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 83.0 µm/m-°C46.1 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 250 °C446 - 482 °F
Middle Barrel Temperature 220 - 240 °C428 - 464 °F
Front Barrel Temperature 210 - 230 °C410 - 446 °F
Nozzle Temperature 240 - 250 °C464 - 482 °F
Melt Temperature 240 - 250 °C464 - 482 °F
Drying Temperature 120 °C248 °F
Dry Time 3 - 5 hour3 - 5 hour
Moisture Content <= 0.020 %<= 0.020 %
Screw Speed 30 - 80 rpm30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Samyang Triloy® 225 PC/ABS alloy
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen)

PSAMY032 / 88114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.