MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PA66-CF40-01-US PA66, 40% Specialty
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: 40% long carbon fiber reinforced Nylon 6/6
40% long carbon fiber reinforced Nylon 6/6

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 290 MPa42100 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.06 %1.06 %5mm/min; ISO 527-2/1A
Tensile Modulus 31.0 GPa4500 ksi1mm/min; ISO 527-2/1A
Flexural Strength 464 MPa67300 psiISO 178
Flexural Modulus 26.0 GPa3770 ksiISO 178
Charpy Impact, Notched 2.40 J/cm²11.4 ft-lb/in²ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 80.0 °C158 - 176 °F
 80.0 - 100 °C176 - 212 °FCavity temperature
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 285 - 295 °C545 - 563 °F
Zone 2 290 - 300 °C554 - 572 °F
Zone 3 300 - 310 °C572 - 590 °F
Zone 4 300 - 315 °C572 - 599 °F
Die Temperature 300 - 315 °C572 - 599 °F
Melt Temperature 300 - 315 °C572 - 599 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content 0.18 %0.18 %Necessary low maximum residual
Dew Point <= -30.0 °C<= -22.0 °FPre-drying
 
Descriptive Properties
Longer pre-drying times/storageMaterial can be over dried and may discolor.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PA66-CF40-02 AF3004 Natural Nylon 66, 40% LCF
Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty
Celanese Celstran® PPS-CF40-01 PPS, 40% Specialty
Celanese Celstran® PBT-CF40-09 PBT, 40% Specialty
Celanese Celstran® PBT-CF40-08 PBT, 40% LCF

PHCR135 / 158704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.