MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery Feel

Color concentrates with polypropylene, ethylene vinyl acetate, or low density polyethylene carriers are most suitable for coloring Dynaflex™ G2730. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have an effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene or polypropylene. Regrind levels up to 20% can be used with Dynaflex™ G2730 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynaflex™ G2730 has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 500 to 700 psi

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.888 g/cc0.888 g/ccASTM D792
Viscosity  5900 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
5900 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
 30700 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
30700 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 252510 sec; ASTM D2240
Tensile Strength at Break 3.03 MPa
@Temperature 23.0 °C
439 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress at Strain 1.21 MPa
@Strain 300 %,
Temperature 23.0 °C
175 psi
@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 650 %
@Temperature 23.0 °C
650 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 - 204 °C379 - 399 °F
Front Barrel Temperature 204 - 216 °C399 - 421 °F
Nozzle Temperature 216 - 232 °C421 - 450 °F
Melt Temperature 179 - 235 °C354 - 455 °F
Mold Temperature 23.9 - 65.6 °C75.0 - 150 °F
Back Pressure 0.689 - 1.38 MPa99.9 - 200 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1210
 
Descriptive Properties
AppearanceTranslucent
FeaturesGood Weather Resistance
 Resilient
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAsia Pacific
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesConsumer Applications
 Overmolding
 Personal Care
 Soft Touch Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G6713C Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G2701C Thermoplastic Elastomer (TPE)

PH0POL1179 / 145748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.