MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® ALR E50D Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Estane® ALR E50D is a clear aliphatic thermoplastic polyurethane (TPU).

Features: Non-yellowing with good mechanical properties.

Available in Americas

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151ASTM D2240
Tensile Strength, Ultimate 57.2 MPa8300 psiASTM D412
Elongation at Break 360 %360 %ASTM D412
100% Modulus 12.4 MPa
@Strain 100 %
1800 psi
@Strain 100 %
ASTM D412
200% Modulus 20.0 MPa
@Strain 200 %
2900 psi
@Strain 200 %
ASTM D412
300% Modulus 38.6 MPa
@Strain 300 %
5600 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0896 GPa13.0 ksiASTM D790

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane
Lubrizol Estane® ALR E87A Thermoplastic Polyurethane
Lubrizol Estane® ALR E60D Thermoplastic Polyurethane
Lubrizol Estane® ALR E65D Thermoplastic Polyurethane

PNOVEON571 / 121462

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.