MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui Milastomer™ 9020NS Natural Vulcanized Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: General Purpose Grade.

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D1505
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  89
@Time 5.00 sec
89
@Time 0.00139 hour
ISO 48
 91
@Time 0.000 sec
91
@Time 0.000 hour
ISO 48
Tensile Strength at Break 8.60 MPa1250 psiJIS No. 3 Dumbbell; 500 mm/min.; ISO 37
Elongation at Break 560 %560 %JIS No. 3 Dumbbell; 500 mm/min.; ISO 37
100% Modulus 5.40 MPa
@Strain 100 %
783 psi
@Strain 100 %
JIS No. 3 Dumbbell; 500 mm/min.; ISO 37
Compression Set  37 %
@Temperature 23.0 °C,
Time 79200 sec
37 %
@Temperature 73.4 °F,
Time 22.0 hour
ISO 815
 58 %
@Temperature 70.0 °C,
Time 79200 sec
58 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °F
 
Descriptive Properties
Major UsesWeather Strip, Gasket
ProcessingExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui Milastomer™ M4400NS Natural Vulcanized Thermoplastic Elastomer
Mitsui Milastomer™ 6010NS Natural Vulcanized Thermoplastic Elastomer
Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Mitsui Milastomer™ 9020BS Black Vulcanized Thermoplastic Elastomer
Mitsui Milastomer™ L900NS Natural Vulcanized Thermoplastic Elastomer

PMIT9940 / 222969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.