MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Tefzel® HT-2160 Static Dissipating Semiconductive Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: DuPont™ Tefzel ® fluoropolymer HT-2160 resin combines the chemical and high-temperature resistance of Tefzel ® with antistatic levels of electrical conductivity. Tefzel ® HT-2160 and the other Tefzel ® fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared to other fluoropolymer resins. They are mechanically tough and offer an excellent balance of properties.

Tefzel ® HT-2160 can perform successfully in applicationswhere other thermoplastics are lacking in mechanical toughness, broad thermal capability, abilityto meet difficult environmental conditions, or limited by fabricating problems.

Properly processed products made from virgin Tefzel ® HT-2160 are inert to most solvents and chemicals, hydrolytically stable, and weather resistant. The recommended upper service temperature is 150°C (302°F); useful properties are retained at cryogenic ranges. Mechanical properties include outstanding impact strength and cut-through and abrasion resistance.

Applications

Tefzel ® HT-2160 resin can be used to manufacture extruded tubing, pipe, and other profiles for hose; linings of components used in the chemical processing industries; industrial film; injection and blow-molded articles requiring superior electrical, chemical, and thermal properties.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Ethylene Tetrafluoroethylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 34.47 MPa4999 psiASTM D3159
Elongation at Break 200 %200 %ASTM D3159
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.0 ohm-cm7.0 ohm-cmmeasured on compression molded plaques. Resistivity is very sensitive to processing techniques; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 - 280 °C491 - 536 °FASTM D3159
Maximum Service Temperature, Air 150 °C302 °F
 
Descriptive Properties
Chemical/Solvent ResistanceExcellent
Weather ResistanceExcellentYears unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Tefzel® 750 Fluoropolymer Resin
Chemours Tefzel® 280 Resin Modified ETFE
Chemours Tefzel® HT-2129 Fluoropolymer Resin
Chemours Tefzel® HT-2127 Fluoropolymer Resin
Chemours Tefzel® 2195 Fluoropolymer Resin

PDU9296 / 33363

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.