MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott N-SF6 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 805254.337
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.37 g/cc0.122 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 2.02.0
Alkali Class, AR 1.01.0
Stain Resistance Class, FR 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 550550.1/20
Modulus of Elasticity 93.0 GPa13500 ksi
Poissons Ratio 0.2620.262
Shear Modulus 37.0 GPa5370 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.00 µm/m-°C
@Temperature -30.0 - 70.0 °C
5.00 µin/in-°F
@Temperature -22.0 - 158 °F
 10.3 µm/m-°C
@Temperature 20.0 - 300 °C
5.72 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.690 J/g-°C0.165 BTU/lb-°F
Thermal Conductivity 0.960 W/m-K6.66 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 589 °C1090 °F
Softening Point 683 °C1260 °FViscosity 107.6 dPa s
Annealing Point 590 °C1090 °FViscosity 1013.0 dPa s
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.80518
@Wavelength 587.6 nm
1.80518
@Wavelength 587.6 nm
nd
 1.81266
@Wavelength 546.1 nm
1.81266
@Wavelength 546.1 nm
ne
Abbe Number 25.1625.16ve
 25.3625.36vd
Optical Dispersion 0.031750.03175nf - nc
 0.0323040.032304nf' - nc'
Transmission, Visible  48 %
@Thickness 10.0 mm,
Wavelength 380 nm
48 %
@Thickness 0.394 in,
Wavelength 380 nm
 85.7 %
@Thickness 10.0 mm,
Wavelength 405 nm
85.7 %
@Thickness 0.394 in,
Wavelength 405 nm
 96.1 %
@Thickness 10.0 mm,
Wavelength 460 nm
96.1 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.2 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.2 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.3 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.3 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  77.6 %
@Thickness 10.0 mm,
Wavelength 2500 nm
77.6 %
@Thickness 0.394 in,
Wavelength 2500 nm
 99.1 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.1 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  4.0 %
@Thickness 10.0 mm,
Wavelength 365 nm
4.0 %
@Thickness 0.394 in,
Wavelength 365 nm
 15.8 %
@Thickness 10.0 mm,
Wavelength 370 nm
15.8 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B0
Climatic Resistance Test CR1
HG4
K (10-6mm2/N)2.82
Phosphate Resistance PR1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-SK16 Glass
Schott N-LAK8 Glass
Schott N-FK5 Glass
Schott N-BK7 Glass
Fused Quartz

CSGS073 / 93407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.