MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 13 Clear, Low Viscosity, Condensation Cure, Liquid Silicone Material for Coating and Potting Applications
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 13 is a clear, low viscosity, two-component, liquid silicone material which cures at room temperature and can be used for coating or potting applications. This material is typically mixed at a ratio of 100:5. Once mixed, the material is self-leveling and will have a useful work-life of approximately two hours. The material will be fully cured after 24 - 48 hours at room temperature. This material can also be vulcanized at elevated temperatures (up to 70°C) to increase the cure speed.

Key Features:

  • Low viscosity
  • Variable cure speed, with mild heat
  • Transparency
  • Room temperature cure
  • Good adhesion with use of a primer

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 g/cc0.850 g/ccUncatalyzed, Quill Cat 12
 0.980 g/cc0.980 g/ccCatalyzed
 0.980 g/cc0.980 g/ccUncatalyzed, QSil 13
Viscosity 15 cP15 cPUncatalyzed, Quill Cat 12
 650 cP650 cPUncatalyzed, QSil 13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1212Catalyzed, 24 hr.
 1818Catalyzed, 48 hr.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FCatalyzed
Minimum Service Temperature, Air -55.0 °C-67.0 °FCatalyzed
 
Processing PropertiesMetricEnglishComments
Gel Time 120 min120 minCatalyzed
 
Descriptive Properties
ColorClear, slight yellowUncatalyzed, Quill Cat 12
 Water whiteUncatalyzed, QSil 13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Foam
Overview of materials for Silicone Rubber
Dymax 3069P Fast Shallow Potting Compound and Sealant
CHT Group QSil 7720 Addition Cure Potting Material
CHT Group QSil 562 Addition Cure Potting Material

PACC2077 / 199465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.