MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 567 Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 567 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive material that is readily repairable.

Key Features:

  • 100% solids
  • Room temperature cure

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccUncatalyzed, QSil 567A
 1.39 g/cc1.39 g/ccUncatalyzed, QSil 567B
Viscosity 1140 cP1140 cPUncatalyzed, QSil 567B
 1500 cP1500 cPUncatalyzed, QSil 567A
 2000 cP
@Temperature 25.0 °C
2000 cP
@Temperature 77.0 °F
Catalyzed
 2500 cP
@Temperature 40.0 °C
2500 cP
@Temperature 104 °F
Catalyzed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858Cure 20 minutes at 150°C
Tensile Strength 2.14 MPa310 psiCure 20 minutes at 150°C
Elongation at Break 85 %85 %Cure 20 minutes at 150°C
Tensile Modulus 0.00293 GPa0.425 ksiYoung's, Cure 20 minutes at 150°C
Tear Strength 3.16 kN/m18.0 pliCure 20 minutes at 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.47e+15 ohm-cm1.47e+15 ohm-cm
Dielectric Constant 3.12
@Frequency 1000 Hz
3.12
@Frequency 1000 Hz
Dissipation Factor 0.00300.0030
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.370 W/m-K2.57 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Cure Time  20.0 min
@Temperature 150 °C
0.333 hour
@Temperature 302 °F
As Tested
 20.0 min
@Temperature 150 °C
0.333 hour
@Temperature 302 °F
As Tested
 
Descriptive Properties
ColorBlackUncatalyzed, QSil 567B
 WhiteUncatalyzed, QSil 567A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemical Concepts Chem-Set™ GE RTV615A/B Silicone Rubber Compound
Dow SYLGARD® PMCP309 Silicone Surfactant
Overview of materials for Silicone Rubber
Master Bond EP3HTFL One Component Thermal Shock and Heat Resistant Epoxy System
Master Bond EP36 High Temperature Resistant, Toughened Epoxy System

PACC2102 / 199490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.