MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shin-Etsu Silicones KE-3611U Electrically Conductive Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: ShinEtsu KE3611 U is a black semi conductive silicone compound. It has been designed as a 60 Durometer material with typical volume resistivity values of 5 W cm.

Product Features:

  • Suitable for both molding and extrusion.
  • Can be catalyzed with both peroxide and addition cure catalysts.
Typical Applications:
  • Key pads.
  • E M I gaskets.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccDBPH Cure
 1.16 g/cc1.16 g/ccDBPH-50 Cure
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565DBPH Cure
 6565DBPH-50 Cure
Tensile Strength at Break 4.71 MPa683 psiDBPH-50 Cure
 4.90 MPa710 psiDBPH Cure
Elongation at Break 290 %290 %DBPH Cure
 320 %320 %DBPH-50 Cure
Tear Strength 11.4 kN/m65.0 pliDie B; DBPH Cure
 11.7 kN/m67.0 pliDie B; DBPH-50 Cure
Compression Set 18 %
@Temperature 180 °C,
Time 79200 sec
18 %
@Temperature 356 °F,
Time 22.0 hour
DBPH Cure
 
Descriptive Properties
Cure AgentDBPH
 DBPH-50
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones FE-341U Fluorosilicone Elastomer
Shin-Etsu Silicones KE-571U Silicone Elastomer
Shin-Etsu Silicones KE-581U Silicone Elastomer
Shin-Etsu Silicones KE-971TU Silicone Elastomer
Freudenberg Hydrolysis-Resistant Polyurethane Elastomer

PSHIN219 / 177730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.