Intex® 131 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain any antioxidant. Key Features: The vulcanized latex shows excellent mechanical properties. Intex® 131 can be blended with natural latex Main Applications: Intex® 131 is mainly used for gel and non-gel foams (medium stiffness), adhesives and bitumen modification. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |