MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Muntz metal, UNS C28000, O61 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Fair to excellent corrosion resistance. Excellent hot formability and forgeability for blanking, forming and bending, hot forging and pressing, hot heading and upsetting, shearing.

Applications: architectural, large nuts and bolts, brazing rod, condenser plates, heat exchanger and condenser tubing, hot forgings.

Test specimen: flat products - 1mm thickness.

Key Words: CDA 280, CZ109, ISO CuZn40, CEN CW509L, yellow metal, 60/40 brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.39 g/cc0.303 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 8080
Tensile Strength, Ultimate 370 MPa53700 psi
Tensile Strength, Yield 145 MPa21000 psi
Elongation at Break 45 %45 %In 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.3460.346
Machinability 40 %40 %UNS C36000 (free-cutting brass) = 100%
Forgeability 90 %90 %
Shear Modulus 39.0 GPa5660 ksi
Shear Strength 275 MPa39900 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000616 ohm-cm0.00000616 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.8 µm/m-°C
@Temperature 20.0 - 300 °C
11.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 123 W/m-K
@Temperature 20.0 °C
854 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 900 - 905 °C1650 - 1660 °F
Solidus 900 °C1650 °F
Liquidus 905 °C1660 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 625 - 800 °C1160 - 1470 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 63 %59 - 63 %
Iron, Fe <= 0.070 %<= 0.070 %
Lead, Pb <= 0.30 %<= 0.30 %
Zinc, Zn 40 %40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Muntz metal, UNS C28000, M20 Temper flat products
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO35 Temper flat products
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO50 Temper rod
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO70 Temper flat products
Lanthanum, La

MC28000b4 / 11153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.