MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm0.0090 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ASTM D2240
Tensile Strength, Ultimate 41.4 MPa6000 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
50% Modulus 9.30 MPa
@Strain 50 %
9.30 MPa
@Strain 50 %
ASTM D412
100% Modulus 12.0 MPa
@Strain 100 %
1740 psi
@Strain 100 %
ASTM D412
300% Modulus 24.8 MPa
@Strain 300 %
3600 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.165 GPa23.9 ksiASTM D790
Tear Strength 114 kN/m650 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 6060H-22 (coarser); ASTM D1044
Compression Set  25 %
@Temperature 25.0 °C,
Time 79200 sec
25 %
@Temperature 77.0 °F,
Time 22.0 hour
Method B; ASTM D395
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
Method B; ASTM D395
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 216 °C390 - 421 °FExtrusion
 204 - 221 °C399 - 430 °FMolding
Mold Temperature 16.0 - 60.0 °C60.8 - 140 °F
Drying Temperature 88.0 - 104 °C190 - 219 °FAir dew point <-40°C
 
Descriptive Properties
Elongation Set After Break (%)80ASTM D412

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane
Lubrizol Estane® R198A-8 Thermoplastic Polyurethane
Lubrizol Estane® S198A Thermoplastic Polyurethane
Lubrizol Estane® R195A Thermoplastic Polyurethane

PNOVEON549 / 121440

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.