MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Universal Wire Works Inconel 625 (AMS 5837) Filler Metal
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Inconel Filler Metal 625 is recommended for gas metal arc and gas tungsten arc welding of nickel base alloys 625 and 601, Incoloy alloys, carbon steels, low alloy steels and stainless steels. This alloy is useful for jet engine applications requiring excellent stress-rupture strength, oxidation resistance to 1200°F, plus outstanding fatigue strength and cryogenic properties. Many engine applications include ducting systems, combustion systems, thrust reverser assemblies, fuel nozzles, afterburner parts and spray bars.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 689 MPa>= 100000 psi
Tensile Strength, Yield >= 414 MPa
@Strain 0.2 %
>= 60000 psi
@Strain 0.2 %
Elongation at Break 30 %30 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.040 %<= 0.040 %
Carbon, C <= 0.10 %<= 0.10 %
Chromium, Cr 21 %21 %
Cobalt, Co <= 1.0 %<= 1.0 %
Iron, Fe <= 5.0 %<= 5.0 %
Molybdenum, Mo 9.0 %9.0 %
Nb + Ta 3.5 %3.5 %
Nickel, Ni 62 %62 %
Titanium, Ti <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK 625 Cast UNS N26625 Severe Corrosion and Heat Resistant Alloy
Special Metals INCONEL® Alloy 625
Special Metals INCONEL® Alloy 718
304 Stainless Steel
Special Metals Nickel 200

NUWW336 / 19754

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.