MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos K44-15-186 Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. It has NSF Standard 14 certification and complies with ANSI/NSF Standard 61 health effects requirements and is recognized by the Plastic Pipe Institute as having a PE 3608 (formerly PE 3408) rating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour>= 5000 hourCondition C; ASTM D1693
ESCR 10% Igepal® >= 2000 hour>= 2000 hourCondition B; ASTM D1693
Melt Flow 12.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 30 hour>= 30 hourNotched Tensile; ASTM F1473
Hardness, Shore D 6868ASTM D2240
Tensile Strength at Break 31.0 MPa4500 psi2 in/min; ASTM D638
Tensile Strength, Yield 22.8 MPa3300 psi2 in/min; ASTM D638
Elongation at Break >= 800 %>= 800 %2 in/min; ASTM D638
Flexural Modulus 0.827 GPa
@Strain 2 %
120 ksi
@Strain 2 %
Secant - Method 1; ASTM D790
Izod Impact, Notched 3.20 J/cm6.00 ft-lb/inASTM D256
Hydrostatic Design Basis 11.0 MPa1600 psiASTM D2837
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -118 °C<= -180 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K44-15-122 HDPE
Ineos G36-24-150 HDPE
Ineos TUB 121N HDPE
ExxonMobil HYA021L High Density Polyethylene Resin
ExxonMobil BA53-055 High Density Polyethylene Resin

PSOLKM021 / 89106

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.