MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NMG ProCell® PC48 PVC Foam Core
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: ProCell® is used in as a core in a variety of composites areas. It can be used in closed molding processes, such hand lay-up and vacuum infusion, etc. ProCell is made mainly from PVC with closed cells and a cross-linked structure. It has extremely high specific strength, specific stiffness and good toughness.

Information provided by NMG Composites Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0480 g/cc0.00173 lb/in³ISO 845
Water Absorption 1.0 %1.0 %ISO 2896
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.03 MPa149 psiASTM–C297
Elongation at Break 12 %12 %Shear elongation; ISO 1922
Tensile Modulus 0.0470 GPa6.82 ksiASTM–C297
Compressive Strength 0.660 MPa95.7 psiASTM- D 1621
Compressive Modulus 0.0450 GPa6.53 ksiASTM- D 1621
Shear Modulus 0.0150 GPa2.18 ksiASTM-C273
Shear Strength 0.690 MPa100 psiASTM-C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0310 W/m-K0.215 BTU-in/hr-ft²-°FISO 8301
 
Descriptive Properties
ColorLilac

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRP - 3/16 - 4.0 Fiberglass/Phenolic Honeycomb
Hexcel® HexWeb® HRH-36 - 1/8 - 2.5 Para-Aramid/Phenolic Core
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb
Evonik Rohacell® 200EC-4 Electrically Conductive Grade Polymethacrylimide (PMI) Foam
Evonik Rohacell® 110 A Aircraft Grade Polymethacrylimide (PMI) Foam

PNMG900 / 230581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.