MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3UG5 BK 23260 25% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Without halogenes and red phosphorus flame retarded 25% glass fiber reinforced injection molding grade; light colorable; outstanding mechanical and electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.1 - 1.5 %1.1 - 1.5 %ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/in
Melt Flow 34.75 g/10 min
@Load 5.00 kg,
Temperature 275 °C
34.75 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psiISO 527-1/-2
Elongation at Break 3.0 %3.0 %ISO 527-1/-2
Modulus of Elasticity 9.50 GPa1380 ksiISO 527-1/-2
Flexural Strength 230 MPa33400 psiISO 178
Flexural Modulus 9.50 GPa1380 ksiISO 178
Charpy Impact Unnotched  6.30 J/cm²
@Temperature -30.0 °C
30.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²
@Temperature 23.0 °C
3.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest Solution A; IEC 60112
Hot Wire Ignition, HWI 0.00 sec
@Thickness >=0.750 mm
0.00 sec
@Thickness >=0.0295 in
ASTM D 3874-88
High Amp Arc Ignition, HAI 0.00 arcs
@Thickness >=0.750 mm
0.00 arcs
@Thickness >=0.0295 in
US 746C
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 527-1/-2
Decomposition Temperature >= 310 °C>= 590 °F
UL RTI, Electrical 120 °C
@Thickness 1.50 mm
248 °F
@Thickness 0.0591 in
UL-746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
Oxygen Index 32 %32 %ISO 4589-1/-2
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
Ignition Temperature >= 350 °C>= 662 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding/Extrusion
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection Molding
 
Descriptive Properties
ColorBK 23260
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Evonik VESTAMID® HTplus M1933 PA6T/X, GF 30
EMS-Grivory Grilon® TSG-30/4 V0 PA666-GF30 FR
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Asahi Kasei Leona™ FH772 Polyamide 66, GF Reinforced, Flame Retardant

PBASG0363 / 131996

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.