MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 65A
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565
Tensile Strength 33.8 MPa4900 psi
Tensile Stress at Strain 33.8 MPa
@Strain 500 %
4900 psi
@Strain 500 %
500% Modulus
Elongation at Break 620 %620 %
100% Modulus 1.90 MPa
@Strain 100 %
275 psi
@Strain 100 %
300% Modulus 9.31 MPa
@Strain 300 %
1350 psi
@Strain 300 %
Tear Strength 43.8 kN/m250 pliGraves
Abrasion 300300NBS Index
Compression Set 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
Method B
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 154 °C
0.500 hour
@Temperature 310 °F
 
Descriptive Properties
Formulation as Tested0.35CAYTUR 4
 0.5Zinc Stearate
 0.75Sulfur
 1MBT
 100Millathane CM
 15Cumar W 2 1/2
 30N330 Carbon Black
 4MBTS
Mooney Scorch>= 30at 250ºF; >30 minutes to a 10 point rise

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Raw Polymer
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Taiwan PU Corporation UR60 Polyester Urethane Rubber
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 287ºF Cure Temperature
Mearthane Durethane™ C 65A Polyurethane

PMILL148 / 87192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.