Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane, Elastomer, Polyester Grade
Material Notes:
Formerly Pellethane
Available in Americas, Europe, Middle East, Africa, India and Asia
Data provided by Lubrizol
Lubrizol acquired the Pellethane product line from Dow in 2009.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.22
g/cc
0.0441
lb/in³
ASTM D792
Linear Mold Shrinkage, Flow
0.0070
-
0.0080
cm/cm
0.0070
-
0.0080
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.0070
cm/cm
0.0070
in/in
ASTM D955
Melt Flow
49
g/10 min
@Load 1.20 kg,
Temperature 224 °C
49
g/10 min
@Load 2.65 lb,
Temperature 435 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
65
65
ASTM D2240
Tensile Strength, Ultimate
44.1
MPa
6400
psi
ASTM D412
Elongation at Break
390 %
390 %
ASTM D412
50% Modulus
16.5
MPa
@Strain 50 %
16.5
MPa
@Strain 50 %
ASTM D412
100% Modulus
20.0
MPa
@Strain 100 %
2900
psi
@Strain 100 %
ASTM D412
300% Modulus
31.0
MPa
@Strain 300 %
4500
psi
@Strain 300 %
ASTM D412
Flexural Modulus
0.255
GPa
37.0
ksi
ASTM D790
Tear Strength
263
kN/m
1500
pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles
120
120
H22 Wheel, 1000 g; ASTM D1044
Compression Set
30 %
@Temperature 25.0 °C,
Time 79200 sec
30 %
@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395, Method B
40 %
@Temperature 70.0 °C,
Time 79200 sec
40 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395, Method B
Tensile Set
110 %
110 %
Elongation set after break; ASTM D412
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
120
µm/m-°C
@Temperature 20.0 °C
66.7
µin/in-°F
@Temperature 68.0 °F
ASTM D696
Vicat Softening Point
142
°C
288
°F
120°C/hr, 9.8N; ASTM D1525
Processing Properties
Metric
English
Comments
Melt Temperature
210
-
221
°C
410
-
430
°F
Molding
Mold Temperature
16.0
-
60.0
°C
60.8
-
140
°F
Drying Temperature
99.0
-
110
°C
210
-
230
°F
air dew point <-40°C
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer
PDW257a / 138253
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.