MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to themselves and to metal glass. Long open and set time ideal for bonding a wide variety of substrates including wood, plastics and also bonds aluminum glass to plastics and wood.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³
Brookfield Viscosity 9000 cP9000 cPThermosel using spindle #27
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545
Tensile Strength at Break 22.8 MPa3310 psiASTM D638 Die C
Elongation at Break 700 %700 %ASTM D638 Die C
Shear Strength  1.90 MPa
@Temperature 82.0 °C
275 psi
@Temperature 180 °F
Overlap, PVC
 2.83 MPa
@Temperature 82.0 °C
410 psi
@Temperature 180 °F
Overlap, Maple
 6.41 MPa
@Temperature 23.0 °C
930 psi
@Temperature 73.4 °F
Overlap, ABS, Substrate Failure
 8.83 MPa
@Temperature 23.0 °C
1280 psi
@Temperature 73.4 °F
Overlap, Polyacrylic, Substrate Failure
 10.3 MPa
@Temperature 23.0 °C
1490 psi
@Temperature 73.4 °F
Overlap, Polycarbonate
 10.8 MPa
@Temperature 23.0 °C
1570 psi
@Temperature 73.4 °F
Overlap, Maple
 11.55 MPa
@Temperature 23.0 °C
1675 psi
@Temperature 73.4 °F
Overlap, PVC
 1.97 MPa
@Time Error in fixSigDigits: @digits must be between 1 a sec
285 psi
@Time Error in fixSigDigits: @digits must be between 1 a hour
Overlap, PVC
 2.83 MPa
@Time Error in fixSigDigits: @digits must be between 1 a sec
410 psi
@Time Error in fixSigDigits: @digits must be between 1 a hour
Overlap, Maple
 3.65 MPa
@Time 3600 sec
530 psi
@Time 1.00 hour
Overlap, PVC
 5.62 MPa
@Time 3600 sec
815 psi
@Time 1.00 hour
Overlap, Maple
 7.93 MPa
@Time 605000 sec
1150 psi
@Time 168 hour
Overlap, Maple
 8.791 MPa
@Time 259000 sec
1275 psi
@Time 72.0 hour
Overlap, Maple
 8.83 MPa
@Time 86400 sec
1280 psi
@Time 24.0 hour
Overlap, Maple
 10.1 MPa
@Time 86400 sec
1460 psi
@Time 24.0 hour
Overlap, PVC
 10.5 MPa
@Time 259000 sec
1530 psi
@Time 72.0 hour
Overlap, PVC
 11.55 MPa
@Time 605000 sec
1675 psi
@Time 168 hour
Overlap, PVC
Peel Strength 8.77 kN/m50.0 pli180°, Polyacrylic
 8.77 kN/m50.0 pli180°, Aluminum
 9.64 kN/m55.0 pli180°, ABS
 10.5 kN/m60.0 pli180°, Glass
 13.1 kN/m75.0 pli180°, PVC, Cotton duck failed during testing
 16.7 kN/m95.0 pli180°, Polycarbonate, Cotton duck failed during testing
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 2.50 min0.0417 hourSet Time
 
Descriptive Properties
Appearancewhite/off-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2644 Z9 POM + PUR
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
BASF Ultraform® N2650 Z4 POM + PUR
BASF Ultraform® N2640 Z2 POM + PUR
Avient OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, PUR

PMM34756 / 169503

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.