MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Manufacturer produces a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industries such as steel, cement, petrochemical and non-ferrous industries.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 2.75 g/cc>= 0.0994 lb/in³Dried at 110°C
Grain Size <= 5000 µm<= 5000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.00735 GPa
@Temperature 1100 °C
1.07 ksi
@Temperature 2010 °F
 0.0118 GPa
@Temperature 110 °C
1.71 ksi
@Temperature 230 °F
 0.0127 GPa
@Temperature 1500 °C
1.84 ksi
@Temperature 2730 °F
Compressive Strength  58.8 MPa
@Temperature 1100 °C
8530 psi
@Temperature 2010 °F
Cold Crushing
 68.6 MPa
@Temperature 1500 °C
9960 psi
@Temperature 2730 °F
Cold Crushing
 93.2 MPa
@Temperature 110 °C
13500 psi
@Temperature 230 °F
Cold Crushing
 34.3 MPa
@Time 86400 sec
4980 psi
@Time 24.0 hour
Cold Crushing
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  1.34 W/m-K
@Temperature 400 °C,
Time 10800 sec
9.30 BTU-in/hr-ft²-°F
@Temperature 752 °F,
Time 3.00 hour
 1.42 W/m-K
@Temperature 600 °C,
Time 10800 sec
9.85 BTU-in/hr-ft²-°F
@Temperature 1110 °F,
Time 3.00 hour
 1.53 W/m-K
@Temperature 800 °C,
Time 10800 sec
10.6 BTU-in/hr-ft²-°F
@Temperature 1470 °F,
Time 3.00 hour
Maximum Service Temperature, Air 1600 °C2910 °F
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 <= 0.70 %<= 0.70 %
 
Descriptive Properties
Permanent Linear Change<-0.05800°C
 <-0.121100°C
 <-0.61500°C
Refractoriness<1750°C
Thermal Expansion0.8Reversible
Water Required to Mix10-12%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Vycor® 7907 UV-Blocking Glass
Chosun Refractories SAL85BR Special High Alumina brick
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet
Chosun Refractories H-4S High Alumina brick
Chosun Refractories H-4 High Alumina brick

CSHARA010 / 130173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.