MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman BMC 1401 Encapsulating Material, Electrical Grade
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for compression molding but excellent in transfer or injection processes. Directly competitive against epoxy encapsulants on cost and cycle times. Very stable shelf life. UL® recognized. This material was formerly known as Glastic® 1401.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.73 - 1.79 g/cc1.73 - 1.79 g/cc
Water Absorption 0.20 - 0.30 %0.20 - 0.30 %24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 40 - 5040 - 50
Tensile Strength, Ultimate 241 - 310 MPa35000 - 45000 psi
Flexural Strength 75.8 - 89.6 MPa11000 - 13000 psi
Flexural Modulus 11.7 - 13.1 GPa1700 - 1900 ksi
Compressive Strength 103 - 117 MPa15000 - 17000 psi
Izod Impact, Notched 0.534 - 1.07 J/cm1.00 - 2.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 11.4 kV/mm290 kV/inShort Time
Dissipation Factor 0.015
@Frequency 60 Hz
0.015
@Frequency 60 Hz
Arc Resistance 190 sec190 sec
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced
A. Schulman BMC 940 Vinyl Ester Bipolar Plate Material
Haysite HCR-196 Corrosion Resistant Vinyl Ester/Glass Sheet
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC

PBMC045 / 27228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.