MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ASTM D792
Water Absorption 0.10 %0.10 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 621 MPa90100 psiASTM D638
Tensile Modulus 21.0 GPa3050 ksiASTM D638
Flexural Strength 690 MPa100000 psiASTM D790
Flexural Modulus 28.0 GPa4060 ksiASTM D790
Compressive Strength 110 MPa16000 psiTransverse; ASTM D695
 414 MPa60000 psiAxial; ASTM D695
Shear Strength 24.0 MPa3480 psiIn-plane. ASTM D3914
Izod Impact, Notched 21.4 J/cm40.1 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 ohm1.00e+14 ohmInsulation Resistance, ASTM D257
Dielectric Constant 5.0
@Frequency 60 Hz
5.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 3.00 kV/mm76.2 kV/in1 in. axial in oil; ASTM D149
Arc Resistance 150 sec150 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 °C
5.00 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 200 °C392 °F
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod
Röchling Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Röchling Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate
Röchling Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester

PGLASK / 41921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.