MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® PA6 900/1 GF20 SV1180-10MCF Nylon 6, 20% glass fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Base Polymer: Polyamide 6

Filler/Additive System: 20% glass fiber

Special Features: metallic effect, low tendency to flow lines

Market Segment: Automotive, Machinery, Electrical and Electronic

Typical Applications: housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Time 86400 sec
0.0020 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
@Time 86400 sec
0.0050 - 0.0080 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 7.20 GPa1040 ksiISO 527
Flexural Strength 185 MPa26800 psiISO 178
Flexural Modulus 6.00 GPa870 ksiISO 178
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-1/-2
Vicat Softening Point 212 °C414 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FInjection molding
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Drying Temperature >= 80.0 °C
@Time 7200 - 43200 sec
>= 176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALCOM® PA6 900/1 GF30 MO2 Nylon 6, 30% glass fiber, 2% molybdenium disulphide reinforced, Dry
Mocom (ALBIS) ALCOM® PA6 900/1 CF10 GF25 IM Nylon 6, 10% carbon fiber, 25% glass fiber
Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA PA66 AE Polyamide 66, extruded
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding

PALBIS8083 / 242142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.