MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Uniprene® 87A Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Features: High Elastic Recovery

Information Provided by Teknor Apex

Key Words: TPV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 87875 seconds; ASTM D2240
Tensile Strength at Break 11.4 MPa1650 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
100% Modulus 6.55 MPa
@Strain 100 %
950 psi
@Strain 100 %
ASTM D412
Tear Strength 56.0 kN/m320 pliDie C; ASTM D624
Compression Set  36 %
@Temperature -5.00 °C,
Time 79200 sec
36 %
@Temperature 23.0 °F,
Time 22.0 hour
Method B; ASTM D395
 50 %
@Temperature 21.1 °C,
Time 79200 sec
50 %
@Temperature 70.0 °F,
Time 22.0 hour
Method B; ASTM D395
 58 %
@Temperature 37.8 °C,
Time 79200 sec
58 %
@Temperature 100 °F,
Time 22.0 hour
Method B; ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers EFLEX® S4040 High Temperature
E-Polymers EFLEX® S4070 High Temperature
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced
Barlog Plastics KEBAFLEX U A 85 HT B01 natural TPU, Shore A85, natural, high temperature resistance

PTEKNO861 / 129042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.