MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic BMC SLC-2000 Glass-Reinforced Polyester BMC, Injection Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.04 g/cc0.0737 lb/in³ASTM D792
Water Absorption 0.090 %0.090 %ASTM D570
Linear Mold Shrinkage 0.0013 cm/cm0.0013 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 28.0 MPa4060 psiASTM D638
Tensile Modulus 15.0 GPa2180 ksiASTM D638
Flexural Strength 94.0 MPa13600 psiASTM D790
Flexural Modulus 13.0 GPa1890 ksiASTM D790
Compressive Strength 152 MPa22000 psiASTM D695
Shear Strength 46.0 MPa6670 psiASTM D732
Izod Impact, Notched 1.50 J/cm2.81 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.73e+15 ohm1.73e+15 ohmInsulation Resistance, Condition A, ASTM D257
Dielectric Constant  5.24
@Frequency 1e+6 Hz
5.24
@Frequency 1e+6 Hz
Condition A, ASTM D150
 7.11
@Frequency 60 Hz
7.11
@Frequency 60 Hz
Condition A, ASTM D150
Dielectric Strength 11.0 kV/mm279 kV/inPerpendicular
Dissipation Factor  0.017
@Frequency 60 Hz
0.017
@Frequency 60 Hz
Condition A, ASTM D150; ASTM D150
 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
Condition A, ASTM D150
Arc Resistance 185 sec185 secASTM D495
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
Flammability, UL94 HBHB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC 6241 Glass Fiber Reinforced Compound
A. Schulman BMC 1000 Thermoset Polyester, Food Grade
A. Schulman BMC 1454 for Injection Molding Circuit Breakers
A. Schulman BMC 350 Thermoset Polyester, Medium Impact
A. Schulman BMC 324 Automotive Grade Molding Compound

PGLASB / 41912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.